egger Arcyl/B Monomer (liquid) emerald, 250 ml

SKU: 33076

Product Description

Colored cold polymerizing acrylic material for the manufacturing of hard, fadeless earmolds. Free of amine and cadmium. Polymerization under pressure at a minimum of 2 bar and a maximum of 6 bar and at a temperature of 40 - 45 °C (104 - 113 °F). Polymerization time: 12 minutes.

Mixing ratio: Monomer : Polymer = 1 : 2
Storage Temperature <30°C
Color: emerald

****Available on request****